08-06-2005, 11:22 PM
|
#1 (permalink)
|
|
Non Member
Offline
|
|
Join Date: May 2003
Posts: 113
|
|
mig welding questions
I am going to be doing some welding on a 46 WDX Power Wagon Cab, looking for any tips for producing a flat weld which wont need much grinding. Using arrgon/Carbon dioxide mix with a .30 wire.(I think) Some of it will be a vertical weld, and I have had the most luck traveling down hill so far, but I am dont have tons of experince welding. My Buddy got me started, and I have found out that grinding down those welds takes for ever!!
so far a clean base metal, and slow wire feed seem to be working the best. is there a pattern to follow that works best at spreading the heat/work puddle out? (circles, zig-zag or some thing else)
Thanks,
Jason
__________________
90, D350, 5 speed, 175,000 miles.
|
|
|
|